With an exceptional firing range, Dover Sand's reputation speaks for itself. Just like the traditional smooth. Vitrifying at cone 10 but looking even more beautiful the hotter it is fired, this clay just looks good.
Dover Sand is Dover with the addition of silica sand for added strength and texture. Perfect for those potters switching between wheel throwing and hand building. Adding silica sand allows you to throw bigger and build larger, without losing the plasticity that Dover brings.
This clay may have crazing issues when paired with cone 6 glazes
Cone: 10
Firing Range: Mid to High-Fire
Clay Type: Stoneware
Texture: Medium Coarseness
Best for: Wheel Throwing
Wet Color: Light Grey
Oxidation Color: White
Reduction Color: Grey to White
Avg. Absorption Rate at Cone 6 (+/- .5%): 3.7%
Avg. Absorption Rate at Cone 10 (Oxidation): 1.4%
Avg. Absorption Rate at Cone 10 (Reduction): 1.25%
Avg. Shrinkage Rate at Cone 6: 11.25%
Avg. Shrinkage Rate at Cone 10: 14%
Image 1: Dover Sand in Oxidation, Cone ^6 (Electric Kiln)
Image 2: Dover Sand in Reduction, Cone ^6 (Gas Kiln)
With an exceptional firing range, Dover Sand's reputation speaks for itself. Just like the traditional smooth. Vitrifying at cone 10 but looking even more beautiful the hotter it is fired, this clay just looks good.
Dover Sand is Dover with the addition of silica sand for added strength and texture. Perfect for those potters switching between wheel throwing and hand building. Adding silica sand allows you to throw bigger and build larger, without losing the plasticity that Dover brings.
This clay may have crazing issues when paired with cone 6 glazes
Cone: 10
Firing Range: Mid to High-Fire
Clay Type: Stoneware
Texture: Medium Coarseness
Best for: Wheel Throwing
Wet Color: Light Grey
Oxidation Color: White
Reduction Color: Grey to White
Avg. Absorption Rate at Cone 6 (+/- .5%): 3.7%
Avg. Absorption Rate at Cone 10 (Oxidation): 1.4%
Avg. Absorption Rate at Cone 10 (Reduction): 1.25%
Avg. Shrinkage Rate at Cone 6: 11.25%
Avg. Shrinkage Rate at Cone 10: 14%
Image 1: Dover Sand in Oxidation, Cone ^6 (Electric Kiln)
Image 2: Dover Sand in Reduction, Cone ^6 (Gas Kiln)